Finden Sie HDPE-Geomembran, LDPE-Geomembran, PVC-Geomembran auf Industry Directory, zuverlässige Hersteller / Lieferant / Fabrik aus China
neue Produkte
Zahlungsart: | L/C, D/P |
---|---|
Minimum der Bestellmenge: | 1000 Bag/Bags |
Spec Properties |
GM0.5 |
GM0.75 |
GM1.0 |
GM1.25 |
GM1.5 |
GM2.0 |
GM2.5 |
Thickness |
0.50mm |
0.75mm |
1.00mm |
1.25mm |
1.50mm |
2.00mm |
2.50mm |
Density ( ≥) |
0.940g/cc |
0.940g/cc |
0.940g/cc |
0.940g/cc |
0.940g/cc |
0.940g/cc |
0.940g/cc |
Tensile Properties ( ≥) ? yield strength ? break strength ? yield elongation ? break elongation |
7 kN/m 10kN/m - 600% |
10 kN/m 15kN/m - 600% |
13 kN/m 20 kN/m 11% 600% |
16 kN/m 25 kN/m 11% 600% |
20 kN/m 30 kN/m 11% 600% |
26 kN/m 40 kN/m 11% 600% |
33kN/m 50kN/m 11% 600% |
Tear Resistance ( ≥) |
56 N |
84 N |
115 N |
140 N |
170 N |
225 N |
280 N |
Puncture Resistance ( ≥) |
120 N |
180 N |
240 N |
300 N |
360 N |
480 N |
600 N |
Carbon Black Content ( ≥) |
2.0-3.0% |
2.0-3.0% |
2.0-3.0% |
2.0-3.0% |
2.0-3.0% |
2.0-3.0% |
2.0-3.0% |
Carbon Black Dispersion ( ≥) |
Note(1) |
Note(1) |
Note(1) |
Note(1) |
Note(1) |
Note(1) |
Note(1) |
Oxidative Induction Time(OIT) Standard OIT ( ≥) |
60 min. |
60 min. |
60 min. |
60 min. |
60 min. |
60 min. |
60 min. |
Area |
Application of Geosynthetics |
Hydraulic | Lagooning and Water Treatment, Ornamental Ponds, Golf Courses Aquaculture and Desalination Water LagoonsTanks, Reservoirs, Liquid WasteFloating Cover SolutionsDrainage and FiltrationShading Cover Solutions |
Environment | Tailing ponds, Leach mining,Landfills,Landfill Capping,Protection against corrosion,Vertical Barriers |
Civil Works | Erosion Control, Secondary Containment, Tunnels,Linear and Surface Works,Consolidation of Margins,Soil Reinforcement,Soil Separation. |
Building | Parkings,Roofing,Soundproofing building |
Produktgruppe : HDPE-Geomembran